Application Method
Mixing Instructions:
Styrobond DP should be mixed on site with water in the ratio of approximately 4 parts Styrobond DP to 1 part water by weight, mixing with a high speed mixer for 3-5 minutes. Allow the material to stand for 10 minutes, remix and use. Mix only enough material for immediate use.
Application Method:
When used as an adhesive, apply to the EPS board and press into place using a level. Do not allow adhesive to skin before fixing in place. When used as an embedding mortar, apply a coat of Styrobond DP mix to the EPS board and embed the mesh using a trowel. Apply another coat of mix to the surface to ensure full cover of the mesh and an overall thickness of approximately 3mm.
Clean tools and equipment with water after use.